【Method of Usage】
1.Delute the concentrate with the mixture solvent {water:methanol or ethanol=1:9}in a suitable proportion
2.Apply the deluted liquid to the electro-chemically grained,anodised and pore-sealed substrate at the solid content of 20-40mg/㎡
3.Dry the substrate adequately and effect the sensitive layer coating
【Miscelaneous】
1、Solid content:30%
2、Packed as 25kg/barrel
【Storage conditions】
Keep in cool and dry places